Due to a flaw caused during furnace heating-up, a 600x200mm crack appeared on a partition of the regenerative chamber, so it was difficult to control furnace pressure and the output and product quality was affected. The crack could not be fixed with traditional hot repairing methods, while it was repaired within two hours with ceramic welding technology of the company.